What each steel actually does in the pocket
Four-point scale · more filled means better · Low, Fair, Good, Excellent
| Steel | Edge holding | Toughness | Rust resistance | Sharpening ease |
|---|---|---|---|---|
3Cr13 est budget stainless | Low | Excellent | Good | Very easy |
8Cr13MoV budget stainless | Low | Good | Good | Very easy |
AR-RPM9 est CJRB spray-form stainless | Fair | Fair | Good | Easy |
440A budget stainless · lower carbon | Fair | Low | Excellent | Easy |
440C budget stainless · higher carbon | Fair | Low | Good | Easy |
14C28N Alleima stainless | Low | Excellent | Excellent | Very easy |
Nitro-V nitrogen-alloyed stainless | Low | Excellent | Good | Very easy |
10Cr15CoMoV est SRM stainless | Fair | Good | Good | Easy |
140Cr est SRM stainless | Good | Good | Fair | Moderate |
VG-10 Japanese stainless | Fair | Fair | Good | Easy (strop) |
D2 semi-stainless tool steel | Good | Low | Low | Moderate |
154CM American stainless | Fair | Low | Good | Easy |
S35VN powder stainless | Good | Fair | Good | Moderate |
S45VN powder stainless | Good | Fair | Good | Moderate |
Elmax powder stainless | Good | Fair | Good | Moderate |
M390 powder stainless | Excellent | Low | Excellent | Hard |
Dots are derived from published metallurgical testing (Knife Steel Nerds), which rates toughness, edge retention and corrosion resistance 0–10 from CATRA cutting tests, unnotched Charpy specimens and saltwater exposure. We map those scores onto four dots across the range covered by the steels on this chart, so the dots compare these steels to each other rather than to every steel that exists. Sharpening ease is not measured by anyone; we derive it inversely from edge retention, which is what actually makes a steel stubborn on a stone.
Marked est — no published test data exists for these; rated from composition and the maker's stated hardness only.
440A and 440C are both shown because knives are very often listed only as “440”, without the grade. On the underlying 0–10 ratings 440C scores higher for edge holding and 440A higher for rust resistance; the two edge scores fall inside the same band here, so the dots show them level while the ratings have 440C a little ahead.
Steel behavior varies with heat treat and blade geometry; heat treat affects real-world performance more than the steel name does.